What is XLPE? Cross-linked polyethylene in power cables
XLPE is cross-linked polyethylene: polyethylene whose long molecules are tied to one another, so that the material becomes one connected network instead of a mass of separate chains. In an HV power cable it is the insulation, the thick natural-coloured wall between the conductor screen and the insulation screen (see the layers of an HV cable). Almost all crosslinkable polyethylene compounds for wire and cable are based on low-density polyethylene (LDPE).
XLPE runs from building wire to transmission cables. Nexans lists it as the insulation of building cables such as XVB, and the Borlink™ grades we supply insulate HV AC cables rated up to 230 kV and EHV AC cables rated above 230 kV.
XLPE vs PE: what crosslinking changes
Ordinary polyethylene is a thermoplastic. Crosslinking joins its molecules; Wikipedia notes that at a crosslinking degree of about 80 % they are connected into a network. The result is chemically a thermoset. Compared with thermoplastic polyethylene it does not melt, behaving more like an elastomer: above its melting point it is rubber-elastic, and it can no longer be processed in the melt.
For a cable, the gain is heat resistance. An IAEA paper on electron-beam processing describes the network as what keeps insulation from dripping off an overheated wire in a short circuit. Nexans gives the maximum conductor temperature in service as 90 °C for XLPE and 70 °C for PVC such as H07V-R, and notes that at the same cross-section you can therefore send more current through the XLPE cable. Wikipedia gives the usual ratings of XLPE-insulated cables as a maximum conductor temperature of 90 °C, an emergency rating of up to 140 °C depending on the standard used, and 250 °C during a short circuit.
| Thermoplastic PE | XLPE | |
|---|---|---|
| Structure | Separate molecules | Molecules connected into a network |
| Above the melting point | Melts | Rubber-elastic, does not melt |
| Processing in the melt | Possible | No longer possible |
The hot set test on XLPE data sheets
The Borlink™ insulation sheets cite IEC 60811-507, “Hot set test for cross-linked materials”, which the IEC describes as typically applying to cross-linkable insulating and sheathing compounds. The sheets report the test at 200 °C under 0.20 MPa, with two results: elongation under load and permanent deformation.
For LE4244S, the typical values are 75 % elongation under load and 5 % permanent deformation, measured on crosslinked specimens; the other three Borlink™ insulation sheets give the same figures. The sheets add that typical data should not be used for specification work.
Three ways to crosslink polyethylene
All three methods start the same way. A hydrogen atom is pulled off a polyethylene chain, leaving a reactive site (a radical), and two chains then link either directly or through a silane bridge. Wikipedia distinguishes four types of crosslinked polyethylene: PE-Xa (peroxide), PE-Xb (silane), PE-Xc (electron beam) and PE-Xd (azo). This guide covers the first three.
| Method | How the links form | Cable example (source) |
|---|---|---|
| Peroxide | A peroxide such as dicumyl peroxide splits into radicals when heated, and the chains bond carbon to carbon | HV cable insulation, degassed to reduce peroxide by-products (Jicable’11) |
| Silane (moisture cure) | Silane groups on the polyethylene react with moisture after extrusion and link the chains through Si–O–Si bridges; a catalyst speeds this up | Low-voltage power cables up to 6 kV (Borealis Visico™) |
| Electron beam (irradiation) | After extrusion, an electron accelerator irradiates the insulation; the links form below the crystalline melting point | Wire insulation and jacketing, for example automotive under-the-hood wire (IAEA) |
Peroxide. In an HV cable line the core is insulated and crosslinked in one continuous run. The cable-line maker Maillefer describes its CCV (catenary) lines as serving power cables from medium to extra-high voltage, and its VCV (vertical) lines as serving high and extra-high voltage. The next section follows peroxide crosslinking through an HV cable line.
Silane. Crosslinking happens after extrusion and is accelerated by heat and moisture. Borealis, for example, sells its Visico™ LE4421/LE4438 as a silane crosslinkable natural compound for low-voltage power cables up to 6 kV: a base material plus a catalyst masterbatch that accelerates the moisture-induced crosslinking, mixed 95 parts to 5.
Electron beam. The IAEA paper calls electron-beam crosslinking of wire and cable insulation one of the most established industrial uses of the technique. It puts the dose needed for polyethylene wire and cable insulation at the order of 100–150 kGy or higher, and its table gives 0.4–3 MeV electrons for wire and cable, with a typical penetration of about 5 mm in material of unit density.
How peroxide XLPE becomes HV cable insulation
The compound. The Borlink™ insulation grades are ready-to-use crosslinkable compounds. Their sheets quote the melt flow rate “without peroxide” and measure tensile and hot set properties on crosslinked specimens.
Extrusion without early curing. The sheets give a melt temperature of 125–135 °C. If a significant amount of peroxide already decomposes in the extruder, crosslinking starts too early. Borealis’s patent application EP 2468813 A1 calls this scorch and links it to inhomogeneity, surface unevenness and possibly discoloration in the cable layers. A 2024 paper by Di et al. notes that cable crosslinking agents need a high decomposition temperature for this reason, and that dicumyl peroxide (DCP) is a commonly used crosslinking agent for XLPE cable insulation in China.
Crosslinking in the tube. The conductor screen, insulation and insulation screen can be extruded together in one pass, known as triple extrusion; the Greek grid operator IPTO’s 400 kV cable specification TD-102/3, for example, requires it. The core then crosslinks in the vulcanizing tube of the CCV or VCV line.
Degassing. Peroxide crosslinking leaves by-products. A Jicable’11 paper by Ericsson and Borealis authors names methane, which has to be removed because of the risk of fire or explosion during handling and installation, and the polar by-products acetophenone and cumyl alcohol, which influence dissipation factor and space charge accumulation. HV cores are therefore degassed. The LS4201S and LS4201EHV sheets list a reduced degassing burden.
The Borlink™ insulation sheets also call cleanliness a critical parameter in the applications the grades are intended for: see why superclean insulation matters.
XLPE density, melting point and electrical properties
Density. All four Borlink™ insulation sheets give a typical base resin density of 922 kg/m³ (0.922 g/cm³). The sheets give the density of the base resin only.
Melting point. Wikipedia contrasts XLPE with thermoplastic polyethylene: it does not melt, behaving more like an elastomer. Its crystals still melt: in DSC tests of four XLPE samples, Di et al. found the main melting peak around 110 °C, with crystallinity of 30–34 %.
Electrical properties. In their Electrical properties tables, all four sheets give typical values of 2.3 for the dielectric constant and 0.0003 for the dissipation factor at 50 Hz, and a DC volume resistivity above 10 PΩ·cm at 23 °C. Their meaning and test methods are covered in how to read a Borlink™ data sheet.
The XLPE we supply
We supply crosslinkable Borlink™ XLPE insulation for HV and EHV AC cables:
- LE4244S and LS4201S, for cables rated up to 230 kV (Um = 245 kV), compared here
- LE4244EHV and LS4201EHV, for cables rated above 230 kV, see choosing XLPE insulation for 500 kV
We also supply the semiconductive compounds for the conductor and insulation screens (LE0592S and LE0500). We do not supply silane-crosslinkable or electron-beam compounds, or compounds for low-voltage cable. Grades and data are on the XLPE insulation page. Core grades are held in our Shanghai warehouse; we confirm availability of a given grade when you inquire.
References
- PDF · Borlink™ LE4244S data sheet · Ed.4, 6 Mar 2026
- PDF · Borlink™ LS4201S data sheet · Ed.6, 5 May 2026
- PDF · Borlink™ LE4244EHV data sheet · Ed.4, 6 Mar 2026
- PDF · Borlink™ LS4201EHV data sheet · Ed.3, 5 May 2026
- STANDARD · IEC 60811-507:2012, Hot set test for cross-linked materials · IEC webstore
- WIKI · Cross-linked polyethylene · Cable ratings; peroxide, silane and irradiation crosslinking
- BRAND · Nexans: cable temperatures · Maximum conductor temperature by insulation
- BRAND · Borealis: Visico™ LE4421 / LE4438 · Silane crosslinkable compound for low-voltage cables
- BRAND · Maillefer: high voltage catenary continuous vulcanizing · CCV lines
- BRAND · Maillefer: high voltage vertical continuous vulcanizing · Vertical lines
- PAPER · Electron beam irradiation applications · S. Sabharwal, IAEA, PAC2013; wire and cable, dose, penetration
- PAPER · Influence of crosslink density on electrical performance and rheological properties of crosslinked polyethylene · Di et al., Polymers 16 (2024) 676; DSC, DCP
- SPEC · IPTO TD-102/3, single-core 400 kV XLPE cables · March 2017; triple extrusion
- PATENT · EP 2468813 A1, scorch resistant polyethylene composition · Borealis; definition of scorch
- PAPER · Distribution of peroxide by-products along degassed XLPE HV cables · Jicable’11 E.7.1.3, Ericsson / Borealis
Related products
- Borlink™ LE4244S · Insulation
- Borlink™ LS4201S · Insulation
- Borlink™ LE4244EHV · Insulation
- Borlink™ LS4201EHV · Insulation
- Borlink™ LE0592S · Semiconductive
- Borlink™ LE0500 · Semiconductive