Chemicals glossary: SBC, resin, rosin and test terms
These are the terms used on the data sheets and grade tables in the polymers and resins section. Each entry gives a plain explanation and points to the matching grades. Grade figures come from producers’ data and are typical values unless a limit is stated. Background sources are listed under References.
- SBC: SBC · SIS · SBS · SIBS · SEBS · SEPS and SEP · SEEPS · SEBSS · functionalized SEBS · diblock · styrene content · linear and radial · oil content
- Hydrocarbon resins: tackifier · C5 · C9 · C5/C9 · DCPD · hydrogenated · pure monomer · indene-coumarone · aliphatic, aromatic, cycloaliphatic · water-white
- Rosin and terpene: rosin · rosin ester · hydrogenated and stabilized rosin · polyterpene · terpene phenolic
- Polyolefins and PIB: EVA · VA content · APAO · EnBA and EMA · Vistamaxx · functionalized polyolefins · PIB
- Tests: softening point · ring and ball · Tg · MFR · Brookfield viscosity · solution viscosity · kinematic viscosity · viscosity index · Gardner color · Hazen color · yellowness index · molecular weight · polydispersity · cloud point · acid and hydroxyl number · bromine and iodine number · flash point · pour point · tensile properties · hardness · needle penetration · Mooney and intrinsic viscosity · typical value
Styrenic block copolymers
Styrenic block copolymer (SBC)
A polymer with polystyrene endblocks and a rubber midblock. The endblocks gather into hard domains that hold the rubber together, so the material is elastic at room temperature and processes like a plastic when heated. Grades: styrenic block copolymers.
SIS
Styrene-isoprene-styrene, with a polyisoprene midblock. Kraton lists it as the softest of its SBC types, and TSRC lists its SIS grades for tape and label adhesives. See SIS grades and SIS vs SBS in adhesives.
SBS
Styrene-butadiene-styrene, with a polybutadiene midblock. Main uses include asphalt modification, footwear and adhesives. See SBS grades, SBS vs SEBS and SBS asphalt modification.
SIBS
A block copolymer whose midblock contains both isoprene and butadiene. The listed grade is Kraton D1171, a clear, sprayable polymer for adhesives. See SIBS.
SEBS
Made by hydrogenating SBS. Hydrogenation saturates the butadiene double bonds and gives an ethylene-butylene midblock with better resistance to heat, UV and ozone. See SEBS grades and SBS vs SEBS.
SEPS and SEP
SEPS is made by hydrogenating SIS and has an ethylene-propylene midblock. SEP is the two-block counterpart, made from a styrene-isoprene diblock. See SEPS grades, SEP grades and the SEPS and SEEPS guide.
SEEPS
A hydrogenated SBC, represented here by the Kuraray SEPTON 4000 series. Kuraray says it offers better tensile strength, oil retention and polyethylene compatibility than SEBS. See SEEPS grades.
SEBSS
The type name used here for Kraton A grades, which are hydrogenated block copolymers. Kraton says they offer better compatibility with more polar chemistries. See SEBSS grades.
Functionalized SEBS
SEBS grafted with maleic anhydride. The polar groups let it bond to polar substrates and work as a compatibilizer or impact modifier. See functionalized SEBS.
Diblock content
The share of two-block (A-B) chains in a polymer. Diblock affects the balance of tack, bond strength, viscosity and mixing. Kraton D1114 has under 1 % diblock and a tensile strength of 32 MPa, and D1113 has 55 % and 8 MPa.
Styrene content
The share of polystyrene in the polymer, written as wt% or as a styrene/rubber ratio such as 19/81. With diblock level and molecular weight, it decides whether an adhesive is soft and tacky or hard and cohesive. Values are listed for each SBC grade.
Linear and radial
Two chain shapes given in the structure column. A linear polymer is a single A-B-A chain, and a radial (star) polymer has (A-B) arms joined at a center. TSRC 4186A is a radial SIS.
Oil content
The percentage of oil already blended into a polymer as supplied. Kraton’s 4000 series are oil-extended grades, and D4433P carries 23 % oil. See SIS grades.
Tackifiers and hydrocarbon resins
Tackifier
A low-molecular-weight resin added to raise tack, usually with a glass transition and softening point above room temperature. The main families are rosin, terpene and hydrocarbon resins. See choosing a tackifier and hydrocarbon resins.
C5 petroleum resin
An aliphatic hydrocarbon resin made from the C5 cracking fraction. It suits SIS, natural rubber and other low-polarity elastomers. See C5 grades and C5 vs C9.
C9 petroleum resin
An aromatic hydrocarbon resin made from the C9 cracking fraction, offered in many softening points. It is used in adhesives, coatings, inks and rubber. See C9 grades.
C5/C9 copolymer resin
An aliphatic resin with an aromatic component built in, which improves compatibility with EVA and other polymers. See C5/C9 grades.
DCPD resin
A resin made by thermal polymerization of dicyclopentadiene, a co-product of steam cracking. It comes in liquid and solid grades, mainly for coatings, inks and construction adhesives. See DCPD grades.
Hydrogenated resin
A hydrocarbon resin treated with hydrogen, which gives light color, good oxidation resistance and low odor. Data sheets may say partially or highly hydrogenated. See hydrogenated resins, hydrogenated C5 resins and the article on hydrogenated resins.
Pure monomer resin
A resin polymerized from pure monomers such as styrene and alpha-methylstyrene (AMS). It is light in color, and some grades are water-white. See pure monomer resins and the article on them.
Indene-coumarone resin
A thermoplastic resin made from indene and coumarone, an aromatic type. Indene occurs in coal-tar fractions. See indene-coumarone grades.
Aliphatic, aromatic, cycloaliphatic
Words for a resin’s chemistry. As shorthand, C5 resins are aliphatic, C9 resins are aromatic and DCPD resins are cycloaliphatic. The balance affects compatibility, and cloud point figures help to show it. See hydrocarbon resins.
Water-white
Colorless or nearly so, like water. Water-white grades include Escorez 5300 and Norsolene W-100. The Hazen scale is meant for liquids at this end of the range.
Rosin and terpene resins
Rosin
A brittle resin from pine trees, made up mainly of resin acids such as abietic acid. It comes from living trees (gum rosin), pine stumps (wood rosin) or the kraft pulping process (tall oil rosin). See rosin and the rosin esters guide.
Rosin ester
Rosin reacted with a polyol, most often pentaerythritol or glycerol. Rosin esters are mainly used as tackifiers for hot-melt and pressure-sensitive adhesives. See rosin ester grades.
Hydrogenated and stabilized rosin
Rosin oxidizes and darkens mainly at the conjugated double bonds of abietic-type acids. Hydrogenation removes those bonds, disproportionation is another stabilizing route, and esters of treated rosin resist oxidation better. See hydrogenated rosin and hydrogenated rosin esters.
Polyterpene
A bio-based resin polymerized from terpenes, the hydrocarbons found in turpentine. It is compatible with polyolefins and the SIS midblock. See polyterpene grades and the article on terpene resins.
Terpene phenolic resin
A resin made from terpene and phenol, with a wide polarity range. High functionality grades suit EVA and other polar polymers, and low polarity grades help SIS, SBS and acrylic PSAs stick to difficult substrates. See terpene phenolic grades.
Polyolefins and polyisobutylene
EVA
A copolymer of ethylene and vinyl acetate, widely used as a hot-melt base polymer. Many of its properties are set by the vinyl acetate content. See EVA grades and EVA vinyl acetate content.
VA and comonomer content
The percentage of comonomer in an olefin copolymer, which for EVA is the vinyl acetate (VA) content. More VA favors adhesion to polar substrates such as paper. ExxonMobil UL 05540EH2 has 39 wt% and UL 00218CC3 has 18 wt%.
APAO
Amorphous poly-alpha-olefin, a low-crystallinity olefin polymer used in hot melts. Compared with similar EVAs it tends to have lower melt viscosity, longer open time and slower set. See APAO grades.
EnBA and EMA
EnBA is an ethylene-n-butyl acrylate copolymer, and EMA is an ethylene-methyl acrylate copolymer. Both are olefin copolymers related to EVA. See EnBA and EMA.
Vistamaxx
ExxonMobil’s propylene-based performance polymers. The company describes its low-viscosity hot-melt type as a propylene elastomer with randomly distributed ethylene. See Vistamaxx grades.
Functionalized polyolefins
Polyethylene or polypropylene with maleic anhydride attached, written Ma-PE and Ma-PP. The anhydride adds polar groups to a non-polar polymer. See functionalized polyolefins.
Polyisobutylene (PIB)
A polymer of isobutene whose form runs from free-flowing liquid to gummy solid as the chains get longer. See polyisobutylene grades and the PIB guide.
Test and data sheet terms
Softening point
The temperature at which a resin reaches a set, arbitrary softness, so the value depends on the test method. See how to read tackifier data.
Ring and ball (R&B)
The common softening point test for resins, described in ASTM E28. A disk of sample in a horizontal ring is heated in a bath until it is forced down 25.4 mm under the weight of a steel ball. Tables marked drop method use a different test, as on some rosin ester grades, so do not compare the two directly.
Glass transition temperature (Tg)
The temperature range over which an amorphous material changes from hard and glassy to soft and rubbery. It is not a melting point, and it lies below the crystalline melting temperature where one exists. See the Tg column on polyterpene grades.
Melt flow rate (MFR), melt index
The mass of molten polymer, in g/10 min, that flows through a standard capillary at a set load and temperature (ASTM D1238, ISO 1133). A higher value means lower melt viscosity and usually lower molecular weight. See EVA grades and SIS grades.
Brookfield viscosity
Viscosity measured with a rotational viscometer, in mPa·s or cP. For hot melts it is taken on the melt at a stated temperature (ASTM D3236), and Kraton’s SBC tables give it on a 25 wt% solution, so check the conditions. See APAO grades.
Solution viscosity
The viscosity of a polymer dissolved at a set concentration, such as 25 wt% in toluene. Compare grades only at the same concentration and solvent. See SIS grades.
Kinematic viscosity
Viscosity found by timing a liquid’s flow under gravity through a calibrated glass capillary (ASTM D445), reported in cSt at a stated temperature. It is the main figure for liquid PIB: PIB 24 has 220 cSt at 100 °C.
Viscosity index
A unitless number for how much a fluid’s viscosity changes with temperature. A higher number means viscosity stays more stable. PIB 24 has 117 and PIB 32 has 165.
Gardner color
A color scale that runs from about 1 (light yellow) to a dark 18, widely used for resins. Readings below 1 are at or near water-white. Many tables state the solution it was read on, such as 50 % in toluene. See C9 grades.
Hazen color (APHA, Pt-Co)
A color scale from 0 (distilled water) to 500 (pale yellow) for nearly colorless liquids. Hazen 500 is just under Gardner 2. See pure monomer resins and polyisobutylene.
Yellowness index (YI)
A number calculated from spectrophotometric data that shows how far a sample has moved from clear or white toward yellow. Escorez tables give it on a 50 % toluene solution. See hydrogenated resins.
Molecular weight (Mn, Mw, Mz)
Polymers contain many chain lengths, so molecular weight is given as averages. Mn counts each molecule equally, Mw gives more weight to larger molecules, and Mz points to the high molecular weight tail. Test conditions differ, so compare values within one producer’s data, as on the hydrocarbon resin pages.
Polydispersity (PDI, Pd)
Mw divided by Mn, which shows how broad the distribution of chain lengths is. The value is at least 1 and approaches 1 as chains become uniform. PIB 24 has 2.4.
Cloud point (DACP, MMAP, OMS)
The temperature at which a heated resin solution turns cloudy on cooling, used to judge compatibility. A higher DACP (diacetone alcohol cloud point) means a less polar resin, and a lower MMAP (mixed methylcyclohexane aniline) means a more aromatic resin. A lower OMS (odorless mineral spirits) value means better aliphatic compatibility; see reading tackifier data and hydrogenated resins.
Acid number and hydroxyl number
Acid number is the mg of KOH needed to neutralize the acidic components in 1 g of sample. Hydroxyl number is a related mg KOH/g figure for hydroxyl groups, found by acetylating the sample. Tables for rosin esters and terpene phenolic resins list them.
Bromine number and iodine number
Both measure unsaturation: the grams of bromine or iodine consumed by 100 g of sample. A higher number means more double bonds. Lanzhou LH90-0 lists a bromine number of ≤ 1, and Cray Valley Wingtack 95 an iodine number of 90.
Flash point and fire point
Flash point is the lowest temperature at which a liquid gives off enough vapor to ignite briefly. Fire point is higher, and there the vapor keeps burning after the ignition source is removed. See the hydrogenated C5 grades, which list both.
Pour point
The temperature below which a liquid loses its flow characteristics. PIB 32 has a pour point of 4 °C.
Tensile strength, 300% modulus, elongation at break
Tensile strength is the stress at break, 300% modulus is the stress at 300 % elongation, and elongation at break is how far the sample stretches before it fails. Set at break is the deformation left after the sample breaks. These are listed for SBS grades and other SBC.
Hardness
Resistance to indentation, measured with a durometer. Shore A is for softer materials and Shore D for harder ones. SBC tables use Shore A or JIS A, as on SEBS grades, so check the scale before comparing.
Needle penetration
The depth a standard needle sinks into a sample, in tenths of a millimeter (dmm). Higher values mean a softer material. APAO grades list it: E1060PL has 35 dmm.
Mooney viscosity and intrinsic viscosity
Mooney viscosity comes from the torque needed to turn a disc in a chamber of rubber, in arbitrary Mooney units. Intrinsic viscosity is a dilute-solution value linked to molar mass. Polyisoprene tables list both: IR309 has 45 and 8 dl/g.
Typical value
A representative test result, not a guaranteed limit. Unless a limit is stated, the figures on these pages are typical values and should not be used as specifications.
Grades and inquiry
To find a grade by material, start at the polymers and resins overview or the brand list. For use-based selection, see applications. We supply these grades. Tell us what you need, and we will reply with suitable options.
References
- ENCYCLOPEDIA · Thermoplastic elastomer · Wikipedia; SBC structure and phase separation
- ENCYCLOPEDIA · Tackifier · Wikipedia; definition and resin families
- ENCYCLOPEDIA · Hot-melt adhesive · Wikipedia; APAO, resins and SBC structure
- ENCYCLOPEDIA · Ethylene-vinyl acetate · Wikipedia; VA content
- ENCYCLOPEDIA · Polyisobutene · Wikipedia; structure and molecular weight
- ENCYCLOPEDIA · Rosin · Wikipedia; sources and composition
- ENCYCLOPEDIA · Terpene · Wikipedia; definition and turpentine
- ENCYCLOPEDIA · Indene · Wikipedia; coal tar and indene/coumarone resins
- ENCYCLOPEDIA · Dicyclopentadiene · Wikipedia; origin in steam cracking
- ENCYCLOPEDIA · Softening point · Wikipedia; definition
- ENCYCLOPEDIA · Glass transition · Wikipedia; definition, relation to melting
- ENCYCLOPEDIA · Melt flow index · Wikipedia; definition and units
- ENCYCLOPEDIA · Viscosity index · Wikipedia; definition
- ENCYCLOPEDIA · Molar mass distribution · Wikipedia; Mn, Mw and Mz
- ENCYCLOPEDIA · Dispersity · Wikipedia; Mw/Mn
- ENCYCLOPEDIA · Acid value · Wikipedia; definition
- ENCYCLOPEDIA · Hydroxyl value · Wikipedia; definition
- ENCYCLOPEDIA · Bromine number · Wikipedia; definition
- ENCYCLOPEDIA · Iodine value · Wikipedia; definition
- ENCYCLOPEDIA · Flash point · Wikipedia; flash point and fire point
- ENCYCLOPEDIA · Pour point · Wikipedia; definition
- ENCYCLOPEDIA · Shore durometer · Wikipedia; Type A and Type D
- ENCYCLOPEDIA · Mooney viscometer · Wikipedia; definition
- ENCYCLOPEDIA · Intrinsic viscosity · Wikipedia; definition
- ENCYCLOPEDIA · Viscometer · Wikipedia; glass capillary and rotational instruments
- TEST GUIDE · Tensile set of elastomers · Intertek; residual elongation
- TEST GUIDE · Asphalt penetration testing · Humboldt; tenths of a millimeter, softer at higher values
- TEST GUIDE · APHA/Pt-Co/Hazen vs Gardner color scales · HunterLab; ranges and crossover
- TEST GUIDE · Yellowness index, ASTM E313 · Intertek; definition
- BRAND · Kraton A · Kraton; polar compatibility
- BRAND · SEPTON · Kuraray; SEP, SEPS, SEEPS and SEBS series
- BRAND · Vistamaxx performance polymer data sheet · ExxonMobil; propylene elastomer description
- TRADE · Styrenic block copolymers · Adhesives & Sealants Industry; styrene content and diblock
- TRADE · Hydrogenated styrenic block copolymers for adhesives and sealants · Adhesives & Sealants Industry; SEBS and hydrogenated resins
- PATENT · US 6,838,510 B2, Resin composition for automotive exterior parts · Defines SEBS, SEPS and SEP
- PATENT · US 9,683,144 B2, Pressure-sensitive adhesive mass for low energy or rough surfaces · DACP and polarity
- PATENT · US 9,593,265 B2, Adhesive composition · Ring-and-ball softening point defined
- PATENT · US 6,605,680 B1, Low color, aromatic modified C5 hydrocarbon resins · MMAP, DACP, Mn, Mw and Mz
- PATENT · US 5,391,670 A, Alkylation resins from polycyclic aromatic compounds · OMS cloud point and MMAP
- PAPER · Increase of rosin ester shelf life: improvement of oxidative stability · Mota et al., Instituto Superior Técnico; rosin esters and stabilization