Rosin esters guide: types, softening point, color, uses
Choose a rosin ester on four points: how the rosin was modified, the softening point, the color, and the fit with the base polymer. Plain esters work with a wide range of polymers. Move to a stabilized or hydrogenated type for better oxidation resistance or color, and to a polymerized type for a higher softening point. The grades are listed under rosin esters and hydrogenated rosin esters.
Values in this guide are typical and are not specifications.
Rosin source and esterification
The source can affect odor, bio-based content varies by grade, and the polyol moves the softening point. Commercial rosin is gum rosin from living pine trees, wood rosin from old pine stumps, or tall oil rosin, a by-product of kraft papermaking, and all three are mainly resin acids, chiefly abietic acid.
If odor matters, ask about the source. A patent on low-odor tall oil esters blames the smell of tall oil rosin on small amounts of organic sulfur compounds left from pulping, and that of gum rosin esters on turpentine residues.
If you have a bio-based target, check the grade. Kraton’s rosin esters, made from pulp and paper by-products, run from 85% for SYLVALITE 2010 to 100% for SYLVATAC RE 85 (EU).
Of the two polyols most used, pentaerythritol gives a higher softening point than glycerol: 107 °C against 89 °C in the same patent’s worked examples, and 106 °C for Foral 105-E against 86 °C for Foral 85-E, made from one hydrogenated rosin, in Synthomer’s drop method table.
Acid number separates a rosin from its ester: hydrogenated rosin Foralyn-E reads 168 and hydrogenated rosin ester Foralyn 90 reads 9. Esterifying converts most of the carboxyl groups, but in the wood rosin process EFSA describes the reaction does not go to completion, so a finished ester keeps some monoesters and free resin acids and still shows an acid number.
Stabilized, hydrogenated and polymerized types
Unmodified rosin has two weak points in adhesives: conjugated double bonds, as in abietic acid, oxidize, and the mix of isomers tends to crystallize. The modified types address these, so choose by the problem you need to solve. The examples below all come from the Synthomer list.
| Type | What is changed | What it gives | Examples |
|---|---|---|---|
| Deodorized rosin ester | Odor components removed | Lower odor | Eastman Ester Gum 8D |
| Stabilized rosin ester | Reactive double bonds reduced | Better color stability and oxidation resistance | Permalyn 5095, Permalyn 6110 |
| Partially hydrogenated rosin ester | Part of the double bonds hydrogenated | Better color retention and high oxidation resistance | Staybelite Ester 10-E, Pentalyn H-E |
| Hydrogenated or highly hydrogenated rosin ester | More of the double bonds hydrogenated | Strong resistance to oxidation and to discoloration from heat or aging | Foralyn 90, Foral 85-E |
| Polymerized rosin ester | Based on polymerized rosin | Higher softening point | Poly-Pale Ester 10, Pentalyn C |
Stabilized is a type name and does not point to one process, so compare grades on their own data. One known route, disproportionation, leaves less abietic acid: a patent on glycerol esters of disproportionated rosin reports better color and color stability and a much slower oxidation rate in storage.
Hydrogenation acts on the double bonds directly, and the degree matters. Synthomer describes highly hydrogenated Foral AX-E as keeping its color better and resisting oxidation more than partially hydrogenated Staybelite rosin. The Foral esters are listed for hot-melt and solvent-based adhesives.
Polymerized rosin is mostly dimer acids: Dymerex softens at 138–151 °C and partly polymerized Poly-Pale at 99–106 °C. Both resist oxidation well and do not crystallize. Among the esters, Poly-Pale Ester 10 softens at 109 °C and Pentalyn C at 126 °C. Unesterified products are listed under rosin, hydrogenated rosin and rosin derivatives.
Softening point
Compare softening points only within one method: resins have no definite melting point, so the figure depends on the test. Ring and ball (ASTM E28) is one method, and Synthomer’s European rosin table uses a drop method, so keep those figures apart.
Kraton’s list runs from liquids to hard resins. SYLVALITE 2010 and SYLVATAC RE 12 are liquids, SYLVATAC RE 25 softens at 30 °C, and the harder grades run from 81 °C up to 120 °C at SYLVALITE 2119. Tg rises with softening point, from −30 °C for SYLVALITE 2010 to 68 °C for SYLVALITE 2119. For how these figures feed into a formula, see reading tackifier data and how to choose a tackifier.
Color and stability
The type name does not fix the color, so check the figure for the grade. In Synthomer’s European table, highly hydrogenated Foral 105-E reads Gardner 5+, hydrogenated Foralyn 110 reads 2, and stabilized Permalyn 6110 reads below 1.
Softening point does not fix it either. SYLVATAC 2098 (98 °C) reads Gardner 4 and SYLVALITE 2100 (99 °C) reads Gardner 1, both in 1:1 toluene. Kraton credits its REvolution technology for the light color and stability of SYLVALITE 2100, 2200 and 9100.
Compare on one scale and one sample state. Gardner is the most common scale, very pale resins may use Hazen, as SYLVALITE 9100 does at 88 Hazen, and some rosin tables use USRG letter grades. A reading in 1:1 toluene is taken on a diluted sample, so it cannot be compared directly with a reading on the neat resin.
Fit with the base polymer
Start from the polymer. Kraton describes its rosin esters as compatible with a broad range of polymers, including high and low VA EVA, acrylics, SBR, SIS and SBS. That covers the family, so narrow by form and listed use. Kraton places solid esters in SBC and EVA adhesives for packaging, PSA and woodworking, and liquid esters in water-based acrylic construction adhesives. Synthomer lists rubber compounds and wax modification for Permalyn 5110-C and Permalyn 7110-C. For starting points by polymer type, see the table in how to choose a tackifier.
Typical uses
These are listed uses for individual grades:
- Packaging and bookbinding hot melts: Permalyn 5095-C and Permalyn 5110-C. See hot-melt adhesives.
- Woodworking and packaging hot melts, coatings and inks: Poly-Pale Ester 10 and Pentalyn C. See coatings and inks.
- Pressure-sensitive adhesives: Pentalyn H-E, and Permalyn 5095-C in hot-melt and solvent-based PSA. See pressure-sensitive adhesives.
- Hot-melt road marking: Permalyn 7110-C. See road marking paint.
- Asphalt modification: Permalyn 5095-C lists this use. See asphalt modification and SBS asphalt modification.
- Waterborne adhesives: Kraton’s AQUATAC tackifier dispersions.
- Hard-to-bond substrates: UNI-TAC 70, a strongly polar modified rosin with a high acid number.
Which type when
Start from the requirement that is hardest to meet:
- Broad polymer fit, no hard color or aging limit: a plain ester.
- Low odor: a deodorized ester such as Eastman Ester Gum 8D-M.
- Color stability and oxidation resistance: a stabilized ester such as Permalyn 5095.
- Oxidation resistance: a partially hydrogenated ester such as Pentalyn H-E.
- Resistance to discoloration from heat or aging: a hydrogenated or highly hydrogenated ester such as Foralyn 90 or Foral 85-E.
- Higher softening point: a pentaerythritol ester, or a polymerized ester such as Pentalyn C.
- A liquid resin: SYLVALITE 2010 or SYLVATAC RE 12.
- Palest color or a bio-based target: choose on the figure for the grade, since the type name fixes neither.
Then test the shortlist in your own polymer and formula before you fix a grade.
Grades and inquiry
Full data is on the rosin and derivatives page and the Kraton and Synthomer brand pages. We supply these grades. Send us your polymer, softening point and color limits, and we will reply with matching grades.
References
- BRAND · Bio-based tackifiers for adhesives · Kraton brochure; feedstocks, rosin ester compatibility and uses, UNI-TAC 70, AQUATAC
- BRAND · Kraton: tackifiers for adhesives · Rosin ester compatibility and uses
- BRAND · Foral AX-E data sheet · Synthomer; hydrogenated rosin, color retention, oxidation resistance
- BRAND · Foral 85-E data sheet · Synthomer; glycerol ester, resistance to oxidation and discoloration
- BRAND · Foral 105-E data sheet · Synthomer; pentaerythritol ester of the same rosin
- BRAND · Dymerex data sheet · Synthomer; dimer acids, oxidation, crystallization
- BRAND · Poly-Pale data sheet · Synthomer; softening point, oxidation, crystallization
- PAPER · EFSA: Re-evaluation of glycerol esters of wood rosin (E 445) · Wood rosin esterification; residual monoesters and resin acids
- PAPER · The ring and ball method of test for softening point of bituminous materials, resins, and similar substances · Walker, Bureau of Standards Journal of Research; principle of the test
- PATENT · US 5,175,250, Stabilized rosin and process for production and use thereof · Conjugated double bonds, oxidation, crystallization, disproportionation
- PATENT · US 4,447,354, Method for making oxidation-stable, light-colored glycerol ester of modified rosin · Effect of disproportionation on color and oxidation
- PATENT · US 5,969,092, Preparation of a tall oil rosin ester with a low odor level · Tall oil sulfur compounds and odor; polyols; example softening points
- WIKI · Rosin · Sources and resin acid composition
- WIKI · Abietic acid · Main component of rosin