Reading tackifier data: softening point, color, cloud points

· Basics

A tackifier data table answers four questions: how hard the resin is (softening point, Tg), how pale it is (color), how large its molecules are (Mn, Mw, Mz) and what it will mix with (cloud points, acid value). Read the test label as carefully as the number, and compare grades inside one table. The same property can be measured several ways, and brands do not all use the same method.

Every example below stays within one brand, for that reason. Figures are typical values from the tables on this site, not specifications, unless a limit is stated.

Softening point and its methods

Resins have no definite melting point. They change gradually from brittle solid to liquid, so softening point is set by an agreed test. The usual one is ring and ball (ASTM E28, ISO 4625): a disk of resin held in a ring and loaded with a ball is heated at a set rate, and the result is the temperature at which it flows through a set distance. ASTM D6493 is an automated ring and ball method, and ASTM D6090 is the Mettler cup and ball method.

What to look for:

  • The method in the column heading. Synthomer lists Foral 85-E at 86 °C in a rosin table that uses a drop method. Compare it only with figures from the same method.
  • Melt viscosity alongside. Softening point tracks viscosity within a series. Synthomer Regalite R1090 softens at 88 °C and lists a 140 °C viscosity of 800. Regalite R1100 softens at 100 °C and lists 2500.

When choosing, a higher softening point generally supports heat resistance, and a lower one gives easier flow. Set the target from what the base polymer and the application temperature need.

Color: Gardner, Hazen and YI

These are different scales, so do not convert between them from a data table.

  • Gardner compares a transparent liquid with numbered glass standards (ASTM D1544, ISO 4630). It was developed for resins, and the scale runs from about 1 to 18, with 18 the darkest. Cray Valley gives Wingtack 95 at 1.7 and Norsolene S-95 at 6.5, both 50% in toluene.
  • Hazen, also called platinum-cobalt or APHA, is a scale for pale liquids (ASTM D1209, ISO 6271). It runs from 0 for water-white to 500. Kraton gives SYLVARES SA 100 at Hazen 15, 1:1 in toluene.
  • Yellowness index (YI) is calculated from instrument color readings (ASTM E313) and suits clear, near-colorless samples. ExxonMobil gives Escorez 1304 at YI 29 and Escorez 5300 at YI ≤1, both 50% in toluene.

Check how the sample was prepared. A reading in 50% toluene is taken on a diluted sample, so it is not the same figure as a reading on the neat resin. Kraton’s rosin ester table has separate columns, so SYLVALITE RE 105L at Gardner 3 (neat) and SYLVATAC RE 103S at Gardner 4 (1:1 in toluene) cannot be read against each other.

Color matters for clear adhesives. Hydrogenation and pure monomer feeds are the two usual routes to a very pale hydrocarbon resin. See hydrogenated hydrocarbon resins.

Molecular weight: Mn, Mw, Mz

A resin is a mix of chain lengths, so one number cannot describe it.

  • Mn is the number average and leans toward the small molecules.
  • Mw is the weight average, where larger molecules count more. It is the usual single figure for average size.
  • Mz gives the heaviest molecules the most weight. Higher Mz generally means lower compatibility.
  • Polydispersity (Pd or Mw/Mn) shows how broad the distribution is.

Synthomer’s Piccotac shows why Mz deserves a look:

Grade Softening point, °C Mn Mw Mz Pd
Piccotac 1095 94 800 1700 3500 2.1
Piccotac 1115 110 1100 3800 15900 3.4

Mn rises modestly, but Mz is several times higher, so expect that grade to behave differently in a blend.

Values also depend on method and calibration, so compare them only inside one table.

Tg

Glass transition temperature marks the change from a hard, glassy state to a rubbery or viscous one. It is usually measured by DSC. A tackifier is a low-molecular-weight material with a high Tg. In a published study of SBS hot-melt PSAs, tackifiers with a higher softening point raised the Tg of the adhesive. A plasticizer does the opposite and lowers it.

Cray Valley grades show the range. Wingtack 10 is a liquid with a softening point of 10 °C and a Tg of -31 °C. Wingtack 95 has a softening point of 98 °C and a Tg of 52 °C. When choosing for a pressure-sensitive adhesive, look at Tg as well as softening point. A trade article on pure monomer resins links a high Tg with more temperature resistance and higher melt viscosity.

Cloud points: DACP, MMAP, OMS

A cloud point is the temperature at which a resin dissolved in a hot solvent mix comes out of solution on cooling. Different solvents show different things:

  • MMAP uses a 1:2 mix of methylcyclohexane and aniline. Lower MMAP means more aromatic content.
  • DACP uses a 1:1 mix of xylene and diacetone alcohol. Lower DACP means higher polarity. Strongly aromatic resins can fall below the limit of the test, so tables print values such as <-40.
  • OMS uses odorless mineral spirits. Within a series of similar aromatic resins it tends to rise with molecular weight.

Synthomer tables run across the whole span:

Grade Listed as DACP, °C MMAP, °C
Piccotac 1095 C5 52 94
Piccotac 8095 C5 38 76
Regalrez 3102 Hydrogenated -15 24
Kristalex 3100 Pure monomer <-50 5
Picco A120 C9 <-40 2

The two Piccotac grades share a category, but the cloud points separate them, and Synthomer describes 8095 as aromatic-modified. OMS rises with Mw in the Picco series: 35 °C on Picco A100 (Mw 930), 65 °C on Picco A120 (Mw 1200) and 94 °C on Picco A140 (Mw 1700).

When choosing, match the resin to the polymer: a high MMAP suits low-polarity polymers such as SIS and polyolefins, and a low MMAP suits styrene-rich or polar ones. See C5 vs C9 hydrocarbon resins and pure monomer resins.

Acid value

Acid value is the milligrams of potassium hydroxide needed to neutralize the acidic groups in 1 g of sample. It is a useful measure for resins because they have no pH of their own. It matters most for rosin esters and rosin, which start as rosin acids.

  • Rosin versus ester. Synthomer lists highly hydrogenated rosin Foral AX-E at 166, and highly hydrogenated rosin ester Foral 85-E at 9.
  • The same split at Kraton. UNI-TAC 70 modified rosin is at 155 mg KOH/g, and SYLVATAC RE 85 (EU) ester is at 4.
  • Hydrocarbon resins. Lanzhou Petrochemical sets a limit of ≤0.5 mg KOH/g for its LH grades.

When choosing, a high acid value marks a polar, reactive resin: Synthomer notes that acidic Dymerex reacts readily with polyalcohols or hydrated lime. Kraton describes UNI-TAC 70 as suited to hard-to-bond substrates. A low value marks a more neutral ester or hydrocarbon.

What to check when choosing

Figure Tells you Check
Softening point Hardness, heat resistance, melt viscosity Method
Color Appearance Scale, neat or in solution
Mn, Mw, Mz Size and spread of the molecules Look at Mz
Tg Glassy to rubbery change, effect on the blend Same method (DSC)
MMAP, DACP, OMS Aromatic content, polarity, relative size Match to the polymer
Acid value Free acid groups, reactivity Rosin or ester

These figures narrow the list, and a trial in your own formulation decides it. For hot melts, see the application page. We supply these grades. Send us your polymer and target figures.