RÜTGERS NOVARES TA 120
RÜTGERS NOVARES TA 120 has a softening point of 115-125 °C, joint highest of the 3 grades listed in this series.
Phenol modified C9 hydrocarbon resins.
Typical values
| Softening point, °C | 115-125 |
|---|---|
| OH content, % | app.1.0 |
| Typical color (Gardner 50% toluene) | 6 |
| Product color (Gardner 50% toluene) | max.9 |
| Description | Phenol modified C9 hydrocarbon resin |
Same series, by softening point (low to high)
Applications of this category
Related articles
Selection
C5 vs C9 hydrocarbon resins: differences and how to choose
How C5 and C9 petroleum resins differ in feedstock, aliphatic or aromatic character and polymer compatibility, and where C5/C9 and DCPD resins fit.
Basics
Chemicals glossary: SBC, resin, rosin and test terms
Plain explanations of terms on polymer and resin data sheets: SBC types, hydrocarbon and rosin resins, EVA, APAO, softening point, color, cloud point.
Selection
How to choose a tackifier: a guide by polymer type
Choose a tackifier by polymer: hydrocarbon, rosin and terpene resins compared on polarity, softening point, color and stability, with a decision table.
Unless stated as limits, values shown are typical values and are not a specification guarantee. Please confirm availability and the current specification of a grade when you inquire. Brand and product names belong to their respective owners.
Tell us the grade or application, and we reply with availability and pricing.